Welder (ITI) – Hands‑on Skills
Topic: Step‑by‑Step Methods for a Welding Process
Audience: ITI welding trainees (Entry‑level).
Goal: Provide a clear, repeatable workflow that covers safety, preparation, execution, and inspection for a typical welding task (e.g., MIG welding a lap joint).
1. Simple Explanation
Welding is a controlled fusion of metals. A step‑by‑step method is a systematic checklist that guarantees consistency, safety, and quality. Think of it as a recipe: each step must be followed in order, and you can’t skip or rush any part.
2. Key Points (Checklist)
| # | Step | What You Do | Why It Matters |
|---|---|---|---|
| S1 | Safety First | • Wear full PPE (helmet, gloves, apron, eye protection). • Verify ventilation. • Keep fire‑resistant blankets nearby. |
Prevents burns, eye injury, and fire. |
| S2 | Equipment Check | • Inspect torch, cable, and power source. • Confirm settings (voltage, wire feed, shielding gas). |
Ensures reliable operation and reduces defects. |
| S3 | Work‑piece Preparation | • Clean surfaces (wire brush, solvent). • Cut to exact dimensions. • Align and clamp. |
Removes contamination and ensures proper fit‑up. |
| S4 | Set Up the Welding Station | • Position the workpiece on the table. • Secure clamps & fixtures. • Set torch angle (usually 15–20° from vertical). |
Provides a stable, repeatable position. |
| S5 | Choose the Right Welding Parameters | • Decide on current, voltage, travel speed, and shielding gas. • Use the welding procedure specification (WPS) if available. |
Controls heat input and bead profile. |
| S6 | Start the Weld | • Initiate arc, start the bead, maintain steady travel. • Keep a consistent torch speed and angle. |
Produces a clean, continuous bead. |
| S7 | Maintain Heat Input | • Monitor bead shape, penetration, and back flash. • Adjust parameters as needed. |
Avoids burn‑through, warping, or lack of fusion. |
| S8 | Cool & Inspect | • Allow part to cool naturally. • Inspect bead for defects (porosity, cracks, undercut). |
Confirms weld quality before final inspection. |
| S9 | Clean & Finish | • Remove slag, clean bead (wire brush). • Apply surface protection if required. |
Improves appearance and protects against corrosion. |
| S10 | Documentation & Feedback | • Record parameters, any issues, and final inspection results. • Review for improvement. |
Builds a knowledge base and supports continuous improvement. |
Tip: Keep a welding logbook; it helps track trends and spot recurring problems.
3. Worked Example
Task: MIG weld a 2‑inch lap joint of 1 mm mild steel (S355) using a 0.8 mm MIG wire.
3.1. Preparation
| Item | Setting | Reason |
|---|---|---|
| Wire | 0.8 mm MIG (ER70S‑6) | Standard for 1 mm steel. |
| Shielding Gas | Argon 75% + CO₂ 25% | Good penetration and bead shape. |
| Voltage | 20 V | Provides moderate heat for thin stock. |
| Wire Feed Speed | 300 m/min | Balanced for 1 mm material. |
| Torch Angle | 15° from vertical | Minimizes spatter. |
| Travel Speed | 200 mm/min | Matches feed rate for steady bead. |
3.2. Step‑by‑Step Execution
| Step | Action | Observation |
|---|---|---|
| S1 | Put on PPE (helmet, gloves, apron). | Safety gear is correctly fitted. |
| S2 | Inspect torch, cable, and machine. | No damage; power supply at 220 V. |
| S3 | Clean joint surfaces with a wire brush. | Surface free of rust and oil. |
| S4 | Clamp the lap joint 1 cm from the edge. | Joint remains square. |
| S5 | Turn on the welder; set parameters as above. | Settings match WPS. |
| S6 | Start the arc, weld from the left side to the right. | Bead forms smoothly, no pull‑back. |
| S7 | Keep torch at 15°; maintain 200 mm/min speed. | Bead is smooth, tapering slightly at the edges. |
| S8 | Stop welding; allow part to cool for 5 min. | No distortion observed. |
| S9 | Inspect bead: gauge for penetrations, check for porosity. | Bead shows full penetration, no defects. |
| S10 | Brush off slag, apply a light coat of primer. | Finish looks clean; ready for next step. |
| S11 | Record the weld parameters and any observations. | Log entry: “No issues; bead quality excellent.” |
3.3. Result
- Quality: Full penetration, bead width 4 mm, no porosity or cracks.
- Compliance: Meets the WPS for 1 mm mild steel lap joint.
- Efficiency: 18 s of actual welding time, 5 s cooling – about 25 s per joint.
4. Quick Revision Summary
- Safety → PPE, ventilation, fire‑resistant blankets.
- Equipment Check → Torch, cable, power source, settings.
- Prep → Clean, cut, clamp.
- Setup →