IIT‑JEE / Competitive Level Study Notes
Hands‑On Skills – Welder (ITI)
Topic: Step‑by‑Step Methods
These notes are written to help you master the methodology of welding – the exact sequence of actions that a welder follows for each type of process (MIG, TIG, SMAW).
The emphasis is on exam‑oriented depth: derivations, key formulae, and common pitfalls that can cause you to lose marks or a poor weld.
1. General Procedure (Applicable to All Processes)
| Step | Action | Key Points |
|---|---|---|
| 1.1 | Job Planning | • Read fabrication drawings & specifications. • Identify required joint type, thickness, material, and weld code. |
| 1.2 | Material & Joint Preparation | • Clean surfaces (remove oil, rust, paint). • Fit‑up: proper gap, bevel, root clearance. • Use clamps or fixtures to hold parts. |
| 1.3 | Equipment Setup | • Select welding machine, power source, electrode or wire, shielding gas. • Check machine parameters (current, voltage, wire feed). |
| 1.4 | Safety Checks | • PPE: helmet, gloves, apron, eye protection, respirator. • Verify ventilation, gas lines, grounding. |
| 1.5 | Pre‑Weld Checks | • Confirm welding parameters using a welding data sheet. • Test a scrap piece (if possible). |
| 1.6 | Welding Process | • Perform the weld following the step‑by‑step method specific to the process. • Maintain constant travel speed, arc length, and angle. |
| 1.7 | Post‑Weld | • Heat‑treat if required (stress relief, normalizing). • Clean slag (TIG), or grind off slag (SMAW). |
| 1.8 | Inspection & Testing | • Visual inspection, dimensional check. • Non‑destructive testing (NDT) if specification demands. |
| 1.9 | Documentation | • Record weld parameters, any deviations, and inspection results. |
Tip: In exams, be ready to convert the above bullet‑list into a paragraph with sub‑headings and illustrations.
2. Step‑by‑Step Method for Specific Welding Processes
We provide a template that covers the critical actions for each process.
Keep this handy when you’re asked: “Explain the step‑by‑step method for MIG welding.”
2.1 MIG (Metal Inert Gas) Welding
| Step | Action | Important Details |
|---|---|---|
| 2.1.1 | Set Machine to MIG Mode | • Select AC or DC depending on material (AC for steel or stainless, DC for aluminum). |
| 2.1.2 | Choose Wire & Gas | • Wire diameter: match to desired penetration (0.8–1.2 mm). • Gas: 75 % Ar + 25 % CO₂ (for steel) or 100 % Ar (for aluminum). |
| 2.1.3 | Adjust Current & Voltage | • Use Heat Input (H) formula (see §4). • Target: H = 1.8–2.5 kJ/mm for typical steel. |
| 2.1.4 | Set Wire Feed Speed | • Approx. Wire feed (mm/min) = 7 × Current (A) for DC. |
| 2.1.5 | Secure Workpiece & Clamp | • Ensure proper clamp pressure to avoid distortion. |
| 2.1.6 | Start Arc | • Hold the tip 1–2 cm from the workpiece. • Use a smooth, controlled motion; keep the arc steady. |
| 2.1.7 | Maintain Travel Speed | • Travel speed = 0.1–0.15 m/min (depends on current & wire). |
| 2.1.8 | Change Direction at Joints | • At 90° corners, approach from the outside of the joint to avoid burn‑through. |
| 2.1.9 | Finish | • Cool gradually; avoid rapid quenching. |
Tricky Point: On steel, over‑current creates a “spatter” zone and can lead to porosity.
2.2 TIG (Tungsten Inert Gas) Welding
| Step | Action | Important Details |
|---|---|---|
| 2.2.1 | Select Tungsten Electrode | • ER‑70S‑6 for steel/SS, C‑ER‑5/16 for aluminum. • Tip angle 30–35°. |
| 2.2.2 | Set Shielding Gas | • 100 % Ar for steel/SS. • 3 % He + 97 % Ar for aluminum (for deeper penetration). |
| 2.2.3 | Adjust Current | • Start at 10–15 % of rated current; gradually increase. |
| 2.2.4 | Feed Flux or Filler | • For SMAW‑like welding: |